[1] 邵建达, 戴亚平, 许乔. 惯性约束聚变激光驱动装置用光学元器件的研究进展[J]. 光学 精密工程, 2016, 24(12):2889-2895. (Shao Jianda, Dai Yaping, Xu Qiao. Progress on optical components for ICF laser facility[J]. Optics and Precision Engineering, 2016, 24(12): 2889-2895 doi: 10.3788/OPE.20162412.2889
[2] Stolz C J. The National Ignition Facility: The world’s largest optical system[C]//Proc of SPIE. 2007, 6834: 683402.
[3] Campbell J H, Hawley-Fedder R A, Stolz C J, et al. NIF optical materials and fabrication technologies: an overview[C]//Proc of SPIE.2004, 5341: 84-101.
[4] 余悦. 邦德激光30 000 W超高功率激光切割机全球首发[OL]. 今日制造与升级, 2019: 36-37.

Yu Yue. The debut of 30 000 W super high power laser cutting machine of Bodor Laser. Manufacture & Upgrading Today, 2019: 36-37
[5] Stolz C J, Thomas M D, Griffin A J. BDS thin film damage competition[C]//Proc of SPIE. 2008: 71320C.
[6] Rudolph W, Emmert L, Sun Z, et al. Laser damage in thin films-What we know and what we don’t[C]//Proc of SPIE. 2013: 888516.
[7] Stolz C J, Sheehan L M, von Gunten M K, et al. Advantages of evaporation of hafnium in a reactive environment formanufacture of high-damage-threshold multilayer coatings by electron-beam-deposition[C]//Advances in Optical Interference Coatings, International Society for Optics and Photonics. 1999, 3738: 318-324.
[8] Andre B, Poupinet L, Ravel G. Evaporation and ion assisted deposition of HfO2 coatings: Some key points for high power laser applications[J]. Journal of Vacuum Science & Technology A: Vacuum, Surfaces, and Films, 2000, 18(5): 2372-2377.
[9] 余振, 张伟丽, 朱瑞, 等. 反应电子束蒸发HfO2薄膜的结构、光学、化学和抗激光损伤特性研究[J]. 中国激光, 2020, 47:0403002. (Yu Zhen, Zhang Weili, Zhu Rui, et al. Studies on optical, structural, chemical and laser damage resistant properties of HfO2 films deposited by reactive electron beam evaporation[J]. Chinese Lasers, 2020, 47: 0403002 doi: 10.3788/CJL202047.0403002
[10] Ristau D, Gross T. Ion beam sputter coatings for laser technology[C]//Proc of SPIE.2005: 596313.
[11] Mende M, Jensen L, Ehlers H, et al. Laser induced damage of pure and mixture material high reflectors for 355 nm and 1064 nm wavelength[C]//Proc of SPIE. 2011: 816821.
[12] Wei Yaowei, Pan Feng , Zhang Qinghua, et al. Atomic layer deposition for fabrication of HfO2/Al2O3 thin films with high laser induced damage thresholds[J]. Nano Express, 2015, 10(44): 1-7.
[13] Jensen, L, Maedebach H, Maula J, et al. Laser induced damage threshold and optical properties of TiO2 and Al2O3-coatings prepared by atomic layer deposition[C]//Proc of SPIE. 2012: 853010.
[14] 刘志超, 郑轶, 潘峰, 等. 1064 nm激光预处理对HfO2/SiO2反射膜损伤形态转化影响研究[J]. 红外与激光工程, 2017, 46:0606003. (Liu Zhichao, Zheng Yi, Pan Feng, et al. Effect of 1064 nm laser conditioning on damage morphology change process on HfO2/SiO2 reflective film[J]. Infrared and Laser Engineering, 2017, 46: 0606003 doi: 10.3788/IRLA201746.0606003
[15] 代福, 杨李茗. HfO2/SiO2多层高反膜激光预处理技术[J]. 强激光与粒子束, 2013, 25(4):929-934. (Dai Fu, Yang Liming. Laser conditioning methods for hafnia silica multilayer high-reflective coatings[J]. High Power Laser and Particle Beams, 2013, 25(4): 929-934 doi: 10.3788/HPLPB20132504.0929
[16] 代福, 杨李茗. 激光预处理中薄膜损伤形貌对预处理效果的影响[J]. 红外与激光工程, 2013, 42(1):190-194. (Dai Fu, Yang Liming. Effects of damaged appearance of coatings on its conditioning during laser conditioning[J]. Infrared and Laser Engineering, 2013, 42(1): 190-194 doi: 10.3969/j.issn.1007-2276.2013.01.035
[17] Tan T, Liu B, Wu Z, et al. Annealing effects on structural, optical properties and laser induced damage threshold of MgF2 thin films[J]. Acta Metall Sin, 2017, 30(1): 73-78. doi: 10.1007/s40195-016-0479-x
[18] Xu Cheng, Dong H, Ma J, et al. Influences of SiO2 protective layers and annealing on the laser-induced damage threshold of Ta2O5 films[J]. Chinese Optics Letters, 2008, 6(3): 228-230. doi: 10.3788/COL20080603.0228
[19] Jena S, Tokas R, Rao K, et al. Annealing effects on microstructure and laser induced damage threshold of HfO2/SiO2 multilayer mirrors[J]. Appl Opt, 2016, 55(22): 6108-6114. doi: 10.1364/AO.55.006108
[20] 许宁, 赵泉, 刘伟, 等. 不同退火温度对HfO2薄膜结构和性能的影响[J]. 硅酸盐通报, 2015, 34(S1):215-217. (Xu Ning, Zhao Quan, Liu Wei, et al. Influence of annealing temperature on structure and properties of hafnium dioxide films[J]. Bulletin of the Chinese Ceramic Society, 2015, 34(S1): 215-217
[21] 田光磊, 黄建兵, 贺洪波, 等. 退火对ZrO2薄膜微结构及激光损伤阈值的影响[J]. 强激光与粒子束, 2005, 17(2):217-221. (Tian Guanglei, Huang Jianbing, He Hongbo, et al. Effect of annealing on microstructure and laser induced damage threshold of ZrO2 coatings[J]. High Power Laser and Particle Beams, 2005, 17(2): 217-221
[22] Xu Cheng, Xiao Qiling, Ma Jianyong, et al. High temperature annealing effect on structure, optical property and laser-induced damage threshold of Ta2O5 films[J]. Appl Surf Sci, 2008, 254(20): 6554-6559. doi: 10.1016/j.apsusc.2008.04.034
[23] 刘浩, 潘峰, 卫耀伟, 等. 缺陷对HfO2薄膜的激光弱吸收与损伤阈值的影响[J]. 应用光学, 2015, 36(2):314-320. (Liu Hao, Pan Feng, Wei Yaowei, et al. Influence of defects in HfO2 film on absorptance and LIDT measurements[J]. Journal of Applied Optics, 2015, 36(2): 314-320 doi: 10.5768/JAO201536.0207004