铜矿高压电脉冲破碎的放电与预富集特性

Discharge and preconcentration characteristics of copper ore fragmented by HVP

  • 摘要: 针对高压电脉冲矿物处理中电源侧累计能量难以完整反映负载端实际放电过程及其与铜矿预富集结果之间关系的问题,采用自研高压电脉冲破碎装置,在累计电容储能相近的条件下,设置单次储能和脉冲次数不同的两种综合脉冲输入工况,对低品位铜矿开展破碎试验。同步测量铜矿—水复合负载端的电压、电流波形,通过瞬时功率积分计算单脉冲负载端沉积能量。结果表明,工况Ⅰ和工况Ⅱ的平均峰值电压分别为83.73 kV和83.34 kV,平均峰值电流分别为3.949 kA和3.590 kA,平均单脉冲负载端沉积能量分别为113.81 J和98.65 J,估算累计负载端沉积能量分别为19.92 kJ和23.68 kJ。两组负载端峰值电压接近,但峰值电流和单脉冲沉积能量存在差异。尽管工况Ⅱ的估算累计负载端沉积能量更高,工况Ⅰ仍表现出更好的铜预富集效果:+1.18~4.75 mm粒级Cu品位达到3.49%,为其加权给料品位0.442%的7.9倍;以40 mm为筛分截断粒度时,可抛除43.82%的粗粒物料,铜损失率仅为4.02%;工况Ⅱ的最高Cu品位为1.876%,最大富集比约为6.2。结果表明,在本文两种综合工况范围内,相近的累计电容储能并未对应完全一致的负载端放电响应,累计负载端沉积能量与铜预富集结果亦未表现出简单一致关系。预富集效果较好的工况同时表现出较高的峰值电流和单脉冲沉积能量,提示除累计能量总量外,单脉冲瞬态放电强度可能也是影响铜矿选择性富集的一个值得进一步关注的因素。

     

    Abstract:
    Background High voltage pulse (HVP) fragmentation has potential for selective breakage and preconcentration of copper ore. However, cumulative capacitor energy at the power source does not fully characterize the electrical response and energy deposition at the ore–water load, making it difficult to relate pulse input conditions to preconcentration outcomes.
    Purpose This study aimed to compare load-side discharge characteristics, energy deposition, and copper preconcentration under two HVP operating conditions with similar cumulative capacitor energy but different energies per pulse and pulse numbers.
    Methods Low-grade copper ore was treated using a self-developed HVP fragmentation system. Condition I employed a charging voltage of 3.0 kV and 175 pulses, whereas Condition II employed 2.5 kV and 240 pulses. Their cumulative capacitor energies were 39.38 and 37.50 kJ, respectively. Load voltage and current were measured synchronously. Twenty pulses sampled across each treatment were analyzed, and deposited energy per pulse was calculated by integrating instantaneous power. Cumulative energy deposited at the load was estimated from the mean sampled value and total pulse number. Fragmentation products were screened and analyzed for Cu grade, recovery, and enrichment.
    Results The average peak voltages under Conditions I and II were 83.73 and 83.34 kV, and the average peak currents were 3.949 and 3.590 kA, respectively. Average deposited energies per pulse were 113.81 and 98.65 J, yielding estimated cumulative load-side deposited energies of 19.92 and 23.68 kJ. Under Condition I, the Cu grade of the +1.18–4.75 mm fraction reached 3.49%, approximately 7.9 times its weighted feed grade of 0.442%. With a screening cut size of 40 mm, 43.82% of the mass could be rejected with a Cu loss of 4.02%. Under Condition II, the maximum Cu grade was 1.876%, with a maximum enrichment ratio of approximately 6.2.
    Conclusions For the two operating conditions studied, similar cumulative capacitor energy did not produce identical load-side discharge responses, and higher estimated cumulative energy deposition did not correspond to better copper preconcentration. Better preconcentration coincided with higher peak current and greater energy deposition per pulse, suggesting that transient single-pulse intensity warrants further investigation. These comparisons do not establish independent causal effects of individual discharge parameters.

     

/